<WorkpieceMaterial>
|
||||
<Name>SUS316</Name>
|
||||
<Note>EN-X5CrNiMo17-12-2; AISI-316; UNS-S31600; JIS-SUS316; DIN-1.4401; GB-022Cr17Ni12Mo2; BS-316S31; AFNOR-Z6CND17-11-02</Note>
|
||||
<ElasticModulus_GPa>193</ElasticModulus_GPa>
|
||||
<CompressiveYieldStrength_MPa>290</CompressiveYieldStrength_MPa>
|
||||
<TensileYieldStrength_MPa>290</TensileYieldStrength_MPa>
|
||||
<ElogationRaioAtBreak>0.45</ElogationRaioAtBreak>
|
||||
<HeatCapacity_JdgK>0.50</HeatCapacity_JdgK>
|
||||
<HeatConductivity_WdmK>16</HeatConductivity_WdmK>
|
||||
<Density_gdcm3>8.0</Density_gdcm3>
|
||||
<PoissonRatio>0.30</PoissonRatio>
|
||||
<FusionLatentHeat_Jdg>260</FusionLatentHeat_Jdg>
|
||||
<MeltingTemperature_C>1400</MeltingTemperature_C>
|
||||
</WorkpieceMaterial>
|
||||