<WorkpieceMaterial>
|
||||
<Name>S50C</Name>
|
||||
<ElasticModulus_GPa>205</ElasticModulus_GPa>
|
||||
<CompressiveYieldStrength_MPa>580</CompressiveYieldStrength_MPa>
|
||||
<TensileYieldStrength_MPa>540</TensileYieldStrength_MPa>
|
||||
<ElogationRaioAtBreak>0.16</ElogationRaioAtBreak>
|
||||
<HeatCapacity_JdgK>0.49</HeatCapacity_JdgK>
|
||||
<HeatConductivity_WdmK>50</HeatConductivity_WdmK>
|
||||
<Density_gdcm3>7.85</Density_gdcm3>
|
||||
<PoissonRatio>0.28</PoissonRatio>
|
||||
<FusionLatentHeat_Jdg>270</FusionLatentHeat_Jdg>
|
||||
<MeltingTemperature_C>1495</MeltingTemperature_C>
|
||||
</WorkpieceMaterial>
|
||||