<CutterMaterial>
|
||||
<Name>WC-Co6-800nm</Name>
|
||||
<Note>Tungsten carbide with 6% cobalt binder and 800nm grain size, offering a balance of hardness and toughness</Note>
|
||||
<ElasticModulus_GPa>620</ElasticModulus_GPa>
|
||||
<TensileStrength_MPa>1550</TensileStrength_MPa>
|
||||
<ThermalExpansionCoefficient_dMK>6.5</ThermalExpansionCoefficient_dMK>
|
||||
<HeatConductivity_WdmK>95</HeatConductivity_WdmK>
|
||||
<HeatCapacity_JdgK>0.28</HeatCapacity_JdgK>
|
||||
<Density_gdcm3>15.0</Density_gdcm3>
|
||||
<PoissonRatio>0.22</PoissonRatio>
|
||||
<MeltingTemperature_K>3143</MeltingTemperature_K>
|
||||
<FusionLatentHeat_Jdg>410</FusionLatentHeat_Jdg>
|
||||
<FrictionCoefficient>0.40</FrictionCoefficient>
|
||||
<TemperatureVsHardnessCurve>
|
||||
<Entry Temperature_K="298">17500</Entry>
|
||||
<Entry Temperature_K="873">14800</Entry>
|
||||
<Entry Temperature_K="1013">12500</Entry>
|
||||
<Entry Temperature_K="1173">10000</Entry>
|
||||
<Entry Temperature_K="1273">10000</Entry>
|
||||
<Entry Temperature_K="1373">10000</Entry>
|
||||
<Entry Temperature_K="1473">10000</Entry>
|
||||
</TemperatureVsHardnessCurve>
|
||||
<TemperatureVsWearCoefficientCurve>
|
||||
<Entry Temperature_K="298">1.19</Entry>
|
||||
<Entry Temperature_K="473">1.86</Entry>
|
||||
<Entry Temperature_K="673">7.10</Entry>
|
||||
<Entry Temperature_K="873">25.70</Entry>
|
||||
<Entry Temperature_K="973">42.30</Entry>
|
||||
<Entry Temperature_K="1073">68.50</Entry>
|
||||
<Entry Temperature_K="1173">95.80</Entry>
|
||||
<Entry Temperature_K="1273">130.00</Entry>
|
||||
<Entry Temperature_K="1373">175.00</Entry>
|
||||
<Entry Temperature_K="1473">230.00</Entry>
|
||||
</TemperatureVsWearCoefficientCurve>
|
||||