<CutterMaterial>
<Name>Al2O3-TiC</Name>
<Note>Alumina ceramic with titanium carbide, offering excellent wear resistance and thermal stability for high-speed machining of cast iron and hardened steels</Note>
<ElasticModulus_GPa>400</ElasticModulus_GPa>
<TensileStrength_MPa>700</TensileStrength_MPa>
<ThermalExpansionCoefficient_dMK>8.5</ThermalExpansionCoefficient_dMK>
<HeatConductivity_WdmK>35</HeatConductivity_WdmK>
<HeatCapacity_JdgK>0.80</HeatCapacity_JdgK>
<Density_gdcm3>4.30</Density_gdcm3>
<PoissonRatio>0.24</PoissonRatio>
<MeltingTemperature_K>2323</MeltingTemperature_K>
<FusionLatentHeat_Jdg>1100</FusionLatentHeat_Jdg>
<FrictionCoefficient>0.32</FrictionCoefficient>
<TemperatureVsHardnessCurve>
<Entry Temperature_K="298">22500</Entry>
<Entry Temperature_K="873">21200</Entry>
<Entry Temperature_K="1013">20100</Entry>
<Entry Temperature_K="1173">18700</Entry>
<Entry Temperature_K="1273">17500</Entry>
<Entry Temperature_K="1373">16200</Entry>
<Entry Temperature_K="1473">14800</Entry>
</TemperatureVsHardnessCurve>
<TemperatureVsWearCoefficientCurve>
<Entry Temperature_K="298">0.65</Entry>
<Entry Temperature_K="473">0.82</Entry>
<Entry Temperature_K="673">1.25</Entry>
<Entry Temperature_K="873">2.10</Entry>
<Entry Temperature_K="973">3.45</Entry>
<Entry Temperature_K="1073">5.80</Entry>
<Entry Temperature_K="1173">9.40</Entry>
<Entry Temperature_K="1273">15.20</Entry>
<Entry Temperature_K="1373">24.50</Entry>
<Entry Temperature_K="1473">38.00</Entry>
</TemperatureVsWearCoefficientCurve>
</CutterMaterial>
@@ -0,0 +1,36 @@
<?xml version="1.0" encoding="utf-8"?>
<CutterMaterial>
<Name>CBN-TiN</Name>
<Note>Cubic Boron Nitride with titanium nitride binder, providing exceptional hardness and thermal stability for machining hardened steels and superalloys</Note>
<ElasticModulus_GPa>680</ElasticModulus_GPa>
<TensileStrength_MPa>900</TensileStrength_MPa>
<ThermalExpansionCoefficient_dMK>4.8</ThermalExpansionCoefficient_dMK>
<HeatConductivity_WdmK>130</HeatConductivity_WdmK>
<HeatCapacity_JdgK>0.65</HeatCapacity_JdgK>
<Density_gdcm3>3.48</Density_gdcm3>
<PoissonRatio>0.18</PoissonRatio>
<MeltingTemperature_K>3273</MeltingTemperature_K>
<FusionLatentHeat_Jdg>1500</FusionLatentHeat_Jdg>
<FrictionCoefficient>0.30</FrictionCoefficient>
<TemperatureVsHardnessCurve>
<Entry Temperature_K="298">28000</Entry>
<Entry Temperature_K="873">26500</Entry>
<Entry Temperature_K="1013">25200</Entry>
<Entry Temperature_K="1173">23800</Entry>
<Entry Temperature_K="1273">22500</Entry>
<Entry Temperature_K="1373">21200</Entry>
<Entry Temperature_K="1473">19800</Entry>
</TemperatureVsHardnessCurve>
<TemperatureVsWearCoefficientCurve>
<Entry Temperature_K="298">0.42</Entry>
<Entry Temperature_K="473">0.56</Entry>
<Entry Temperature_K="673">0.85</Entry>
<Entry Temperature_K="873">1.45</Entry>
<Entry Temperature_K="973">2.20</Entry>
<Entry Temperature_K="1073">3.40</Entry>
<Entry Temperature_K="1173">5.20</Entry>
<Entry Temperature_K="1273">8.10</Entry>
<Entry Temperature_K="1373">12.60</Entry>
<Entry Temperature_K="1473">19.80</Entry>
</TemperatureVsWearCoefficientCurve>
</CutterMaterial>
@@ -0,0 +1,36 @@
<?xml version="1.0" encoding="utf-8"?>
<CutterMaterial>
<Name>High-Speed Steel (HSS) - M2</Name>
<Note>The most widely used industrial high-speed steel, offering high wear resistance and toughness.</Note>
<ElasticModulus_GPa>210</ElasticModulus_GPa>
<TensileStrength_MPa>3100</TensileStrength_MPa>
<ThermalExpansionCoefficient_dMK>11.0</ThermalExpansionCoefficient_dMK>
<HeatConductivity_WdmK>24.6</HeatConductivity_WdmK>
<HeatCapacity_JdgK>0.46</HeatCapacity_JdgK>
<Density_gdcm3>8.05</Density_gdcm3>
<PoissonRatio>0.30</PoissonRatio>
<MeltingTemperature_K>1723</MeltingTemperature_K>
<FusionLatentHeat_Jdg>270</FusionLatentHeat_Jdg>
<FrictionCoefficient>0.4</FrictionCoefficient>
<TemperatureVsHardnessCurve>
<Entry Temperature_K="298">8500</Entry>
<Entry Temperature_K="873">7000</Entry>
<Entry Temperature_K="1013">5133</Entry>
<Entry Temperature_K="1173">3000</Entry>
<Entry Temperature_K="1273">3000</Entry>
<Entry Temperature_K="1373">3000</Entry>
<Entry Temperature_K="1473">3000</Entry>
</TemperatureVsHardnessCurve>
<TemperatureVsWearCoefficientCurve>
<Entry Temperature_K="298">1.80</Entry>
<Entry Temperature_K="473">2.50</Entry>
<Entry Temperature_K="673">5.00</Entry>
<Entry Temperature_K="873">15.00</Entry>
<Entry Temperature_K="973">25.00</Entry>
<Entry Temperature_K="1073">40.00</Entry>
<Entry Temperature_K="1173">65.00</Entry>
<Entry Temperature_K="1273">95.00</Entry>
<Entry Temperature_K="1373">140.00</Entry>
<Entry Temperature_K="1473">200.00</Entry>
</TemperatureVsWearCoefficientCurve>
</CutterMaterial>
@@ -0,0 +1,36 @@
<?xml version="1.0" encoding="utf-8"?>
<CutterMaterial>
<Name>High-Speed Steel (HSS) - M35</Name>
<Note>Cobalt-enriched high-speed steel with improved heat resistance and red hardness compared to M2</Note>
<ElasticModulus_GPa>215</ElasticModulus_GPa>
<TensileStrength_MPa>3300</TensileStrength_MPa>
<ThermalExpansionCoefficient_dMK>10.8</ThermalExpansionCoefficient_dMK>
<HeatConductivity_WdmK>25.0</HeatConductivity_WdmK>
<HeatCapacity_JdgK>0.45</HeatCapacity_JdgK>
<Density_gdcm3>8.10</Density_gdcm3>
<PoissonRatio>0.30</PoissonRatio>
<MeltingTemperature_K>1723</MeltingTemperature_K>
<FusionLatentHeat_Jdg>275</FusionLatentHeat_Jdg>
<FrictionCoefficient>0.39</FrictionCoefficient>
<TemperatureVsHardnessCurve>
<Entry Temperature_K="298">9000</Entry>
<Entry Temperature_K="873">7500</Entry>
<Entry Temperature_K="1013">5500</Entry>
<Entry Temperature_K="1173">3500</Entry>
<Entry Temperature_K="1273">3500</Entry>
<Entry Temperature_K="1373">3500</Entry>
<Entry Temperature_K="1473">3500</Entry>
</TemperatureVsHardnessCurve>
<TemperatureVsWearCoefficientCurve>
<Entry Temperature_K="298">1.70</Entry>
<Entry Temperature_K="473">2.30</Entry>
<Entry Temperature_K="673">4.50</Entry>
<Entry Temperature_K="873">12.00</Entry>
<Entry Temperature_K="973">22.00</Entry>
<Entry Temperature_K="1073">35.00</Entry>
<Entry Temperature_K="1173">55.00</Entry>
<Entry Temperature_K="1273">85.00</Entry>
<Entry Temperature_K="1373">125.00</Entry>
<Entry Temperature_K="1473">180.00</Entry>
</TemperatureVsWearCoefficientCurve>
</CutterMaterial>
@@ -0,0 +1,36 @@
<?xml version="1.0" encoding="utf-8"?>
<CutterMaterial>
<Name>High-Speed Steel (HSS) - M42</Name>
<Note>Premium high-speed steel with high cobalt content (8-10%), offering superior hot hardness and wear resistance</Note>
<ElasticModulus_GPa>220</ElasticModulus_GPa>
<TensileStrength_MPa>3500</TensileStrength_MPa>
<ThermalExpansionCoefficient_dMK>10.5</ThermalExpansionCoefficient_dMK>
<HeatConductivity_WdmK>25.5</HeatConductivity_WdmK>
<HeatCapacity_JdgK>0.44</HeatCapacity_JdgK>
<Density_gdcm3>8.20</Density_gdcm3>
<PoissonRatio>0.29</PoissonRatio>
<MeltingTemperature_K>1723</MeltingTemperature_K>
<FusionLatentHeat_Jdg>280</FusionLatentHeat_Jdg>
<FrictionCoefficient>0.38</FrictionCoefficient>
<TemperatureVsHardnessCurve>
<Entry Temperature_K="298">9500</Entry>
<Entry Temperature_K="873">8000</Entry>
<Entry Temperature_K="1013">6000</Entry>
<Entry Temperature_K="1173">4000</Entry>
<Entry Temperature_K="1273">4000</Entry>
<Entry Temperature_K="1373">4000</Entry>
<Entry Temperature_K="1473">4000</Entry>
</TemperatureVsHardnessCurve>
<TemperatureVsWearCoefficientCurve>
<Entry Temperature_K="298">1.60</Entry>
<Entry Temperature_K="473">2.10</Entry>
<Entry Temperature_K="673">4.00</Entry>
<Entry Temperature_K="873">10.00</Entry>
<Entry Temperature_K="973">18.00</Entry>
<Entry Temperature_K="1073">30.00</Entry>
<Entry Temperature_K="1173">48.00</Entry>
<Entry Temperature_K="1273">75.00</Entry>
<Entry Temperature_K="1373">110.00</Entry>
<Entry Temperature_K="1473">160.00</Entry>
</TemperatureVsWearCoefficientCurve>
</CutterMaterial>
@@ -0,0 +1,36 @@
<?xml version="1.0" encoding="utf-8"?>
<CutterMaterial>
<Name>WC-Co10-600nm</Name>
<Note>Tungsten carbide with 10% cobalt binder and 600nm grain size, offering improved toughness for interrupted cutting</Note>
<ElasticModulus_GPa>580</ElasticModulus_GPa>
<TensileStrength_MPa>1680</TensileStrength_MPa>
<ThermalExpansionCoefficient_dMK>7.1</ThermalExpansionCoefficient_dMK>
<HeatConductivity_WdmK>85</HeatConductivity_WdmK>
<HeatCapacity_JdgK>0.27</HeatCapacity_JdgK>
<Density_gdcm3>14.5</Density_gdcm3>
<PoissonRatio>0.23</PoissonRatio>
<MeltingTemperature_K>3123</MeltingTemperature_K>
<FusionLatentHeat_Jdg>390</FusionLatentHeat_Jdg>
<FrictionCoefficient>0.42</FrictionCoefficient>
<TemperatureVsHardnessCurve>
<Entry Temperature_K="298">16200</Entry>
<Entry Temperature_K="873">13600</Entry>
<Entry Temperature_K="1013">11400</Entry>
<Entry Temperature_K="1173">9200</Entry>
<Entry Temperature_K="1273">9200</Entry>
<Entry Temperature_K="1373">9200</Entry>
<Entry Temperature_K="1473">9200</Entry>
</TemperatureVsHardnessCurve>
<TemperatureVsWearCoefficientCurve>
<Entry Temperature_K="298">1.35</Entry>
<Entry Temperature_K="473">2.10</Entry>
<Entry Temperature_K="673">7.80</Entry>
<Entry Temperature_K="873">28.40</Entry>
<Entry Temperature_K="973">46.70</Entry>
<Entry Temperature_K="1073">74.20</Entry>
<Entry Temperature_K="1173">103.50</Entry>
<Entry Temperature_K="1273">142.00</Entry>
<Entry Temperature_K="1373">190.50</Entry>
<Entry Temperature_K="1473">250.00</Entry>
</TemperatureVsWearCoefficientCurve>
</CutterMaterial>
@@ -0,0 +1,36 @@
<?xml version="1.0" encoding="utf-8"?>
<CutterMaterial>
<Name>WC-Co6-500nm-Advanced</Name>
<Note>Advanced tungsten carbide with 6% cobalt binder, 500nm grain size, and optimized properties</Note>
<ElasticModulus_GPa>640</ElasticModulus_GPa>
<TensileStrength_MPa>1580</TensileStrength_MPa>
<ThermalExpansionCoefficient_dMK>6.4</ThermalExpansionCoefficient_dMK>
<HeatConductivity_WdmK>98</HeatConductivity_WdmK>
<HeatCapacity_JdgK>0.28</HeatCapacity_JdgK>
<Density_gdcm3>15.1</Density_gdcm3>
<PoissonRatio>0.21</PoissonRatio>
<MeltingTemperature_K>3173</MeltingTemperature_K>
<FusionLatentHeat_Jdg>420</FusionLatentHeat_Jdg>
<FrictionCoefficient>0.38</FrictionCoefficient>
<TemperatureVsHardnessCurve>
<Entry Temperature_K="298">18700</Entry>
<Entry Temperature_K="873">16200</Entry>
<Entry Temperature_K="1013">14100</Entry>
<Entry Temperature_K="1173">11800</Entry>
<Entry Temperature_K="1273">11800</Entry>
<Entry Temperature_K="1373">11800</Entry>
<Entry Temperature_K="1473">11800</Entry>
</TemperatureVsHardnessCurve>
<TemperatureVsWearCoefficientCurve>
<Entry Temperature_K="298">0.92</Entry>
<Entry Temperature_K="473">1.45</Entry>
<Entry Temperature_K="673">5.80</Entry>
<Entry Temperature_K="873">19.40</Entry>
<Entry Temperature_K="973">32.60</Entry>
<Entry Temperature_K="1073">51.80</Entry>
<Entry Temperature_K="1173">74.50</Entry>
<Entry Temperature_K="1273">105.00</Entry>
<Entry Temperature_K="1373">145.00</Entry>
<Entry Temperature_K="1473">195.00</Entry>
</TemperatureVsWearCoefficientCurve>
</CutterMaterial>
@@ -0,0 +1,36 @@
<?xml version="1.0" encoding="utf-8"?>
<CutterMaterial>
<Name>WC-Co6-800nm</Name>
<Note>Tungsten carbide with 6% cobalt binder and 800nm grain size, offering a balance of hardness and toughness</Note>
<ElasticModulus_GPa>620</ElasticModulus_GPa>
<TensileStrength_MPa>1550</TensileStrength_MPa>
<ThermalExpansionCoefficient_dMK>6.5</ThermalExpansionCoefficient_dMK>
<HeatConductivity_WdmK>95</HeatConductivity_WdmK>
<HeatCapacity_JdgK>0.28</HeatCapacity_JdgK>
<Density_gdcm3>15.0</Density_gdcm3>
<PoissonRatio>0.22</PoissonRatio>
<MeltingTemperature_K>3143</MeltingTemperature_K>
<FusionLatentHeat_Jdg>410</FusionLatentHeat_Jdg>
<FrictionCoefficient>0.40</FrictionCoefficient>
<TemperatureVsHardnessCurve>
<Entry Temperature_K="298">17500</Entry>
<Entry Temperature_K="873">14800</Entry>
<Entry Temperature_K="1013">12500</Entry>
<Entry Temperature_K="1173">10000</Entry>
<Entry Temperature_K="1273">10000</Entry>
<Entry Temperature_K="1373">10000</Entry>
<Entry Temperature_K="1473">10000</Entry>
</TemperatureVsHardnessCurve>
<TemperatureVsWearCoefficientCurve>
<Entry Temperature_K="298">1.19</Entry>
<Entry Temperature_K="473">1.86</Entry>
<Entry Temperature_K="673">7.10</Entry>
<Entry Temperature_K="873">25.70</Entry>
<Entry Temperature_K="973">42.30</Entry>
<Entry Temperature_K="1073">68.50</Entry>
<Entry Temperature_K="1173">95.80</Entry>
<Entry Temperature_K="1273">130.00</Entry>
<Entry Temperature_K="1373">175.00</Entry>
<Entry Temperature_K="1473">230.00</Entry>
</TemperatureVsWearCoefficientCurve>
</CutterMaterial>
@@ -0,0 +1,36 @@
<?xml version="1.0" encoding="utf-8"?>
<CutterMaterial>
<Name>WC-Co6-TiC-400nm</Name>
<Note>Tungsten carbide with 6% cobalt binder, TiC addition, and 400nm grain size, offering enhanced wear resistance and thermal stability</Note>
<ElasticModulus_GPa>650</ElasticModulus_GPa>
<TensileStrength_MPa>1600</TensileStrength_MPa>
<ThermalExpansionCoefficient_dMK>6.2</ThermalExpansionCoefficient_dMK>
<HeatConductivity_WdmK>100</HeatConductivity_WdmK>
<HeatCapacity_JdgK>0.29</HeatCapacity_JdgK>
<Density_gdcm3>15.2</Density_gdcm3>
<PoissonRatio>0.20</PoissonRatio>
<MeltingTemperature_K>3193</MeltingTemperature_K>
<FusionLatentHeat_Jdg>430</FusionLatentHeat_Jdg>
<FrictionCoefficient>0.36</FrictionCoefficient>
<TemperatureVsHardnessCurve>
<Entry Temperature_K="298">19200</Entry>
<Entry Temperature_K="873">17100</Entry>
<Entry Temperature_K="1013">15300</Entry>
<Entry Temperature_K="1173">13200</Entry>
<Entry Temperature_K="1273">13200</Entry>
<Entry Temperature_K="1373">13200</Entry>
<Entry Temperature_K="1473">13200</Entry>
</TemperatureVsHardnessCurve>
<TemperatureVsWearCoefficientCurve>
<Entry Temperature_K="298">0.85</Entry>
<Entry Temperature_K="473">1.32</Entry>
<Entry Temperature_K="673">5.10</Entry>
<Entry Temperature_K="873">17.60</Entry>
<Entry Temperature_K="973">29.30</Entry>
<Entry Temperature_K="1073">46.50</Entry>
<Entry Temperature_K="1173">68.20</Entry>
<Entry Temperature_K="1273">95.00</Entry>
<Entry Temperature_K="1373">130.00</Entry>
<Entry Temperature_K="1473">175.00</Entry>
</TemperatureVsWearCoefficientCurve>
</CutterMaterial>
@@ -0,0 +1,36 @@
<?xml version="1.0" encoding="utf-8"?>
<CutterMaterial>
<n>WC</n>
<Note>Pure tungsten carbide without binder, offering extreme hardness but limited toughness</Note>
<ElasticModulus_GPa>700</ElasticModulus_GPa>
<TensileStrength_MPa>1200</TensileStrength_MPa>
<ThermalExpansionCoefficient_dMK>5.5</ThermalExpansionCoefficient_dMK>
<HeatConductivity_WdmK>110</HeatConductivity_WdmK>
<HeatCapacity_JdgK>0.25</HeatCapacity_JdgK>
<Density_gdcm3>15.6</Density_gdcm3>
<PoissonRatio>0.19</PoissonRatio>
<MeltingTemperature_K>3143</MeltingTemperature_K>
<FusionLatentHeat_Jdg>450</FusionLatentHeat_Jdg>
<FrictionCoefficient>0.35</FrictionCoefficient>
<TemperatureVsHardnessCurve>
<Entry Temperature_K="298">20000</Entry>
<Entry Temperature_K="873">18000</Entry>
<Entry Temperature_K="1013">16000</Entry>
<Entry Temperature_K="1173">14000</Entry>
<Entry Temperature_K="1273">14000</Entry>
<Entry Temperature_K="1373">14000</Entry>
<Entry Temperature_K="1473">14000</Entry>
</TemperatureVsHardnessCurve>
<TemperatureVsWearCoefficientCurve>
<Entry Temperature_K="298">1.19</Entry>
<Entry Temperature_K="473">1.86</Entry>
<Entry Temperature_K="673">7.10</Entry>
<Entry Temperature_K="873">25.70</Entry>
<Entry Temperature_K="973">42.30</Entry>
<Entry Temperature_K="1073">68.50</Entry>
<Entry Temperature_K="1173">95.80</Entry>
<Entry Temperature_K="1273">130.00</Entry>
<Entry Temperature_K="1373">175.00</Entry>
<Entry Temperature_K="1473">230.00</Entry>
</TemperatureVsWearCoefficientCurve>
</CutterMaterial>