<?xml version="1.0" encoding="utf-8"?>
|
||||
<CoatingMaterial>
|
||||
<Name>TiCN</Name>
|
||||
<Note>Titanium Carbonitride Coating</Note>
|
||||
<ElasticModulus_GPa>420</ElasticModulus_GPa>
|
||||
<TensileStrength_MPa>1150</TensileStrength_MPa>
|
||||
<ThermalExpansionCoefficient_dMK>8.5</ThermalExpansionCoefficient_dMK>
|
||||
<HeatConductivity_WdmK>27</HeatConductivity_WdmK>
|
||||
<HeatCapacity_JdgK>0.52</HeatCapacity_JdgK>
|
||||
<Density_gdcm3>5.0</Density_gdcm3>
|
||||
<PoissonRatio>0.25</PoissonRatio>
|
||||
<PreferedThickness_um>2</PreferedThickness_um>
|
||||
<MeltingTemperature_K>3173</MeltingTemperature_K>
|
||||
<FusionLatentHeat_Jdg>370</FusionLatentHeat_Jdg>
|
||||
<FrictionCoefficient>0.38</FrictionCoefficient>
|
||||
<TemperatureVsHardnessCurve>
|
||||
<Entry Temperature_K="298.16">24000</Entry>
|
||||
<Entry Temperature_K="873.16">20000</Entry>
|
||||
<Entry Temperature_K="1073.16">16000</Entry>
|
||||
<Entry Temperature_K="1273.16">12000</Entry>
|
||||
</TemperatureVsHardnessCurve>
|
||||
<TemperatureVsWearCoefficientCurve>
|
||||
<Entry Temperature_K="298.16">0.95</Entry>
|
||||
<Entry Temperature_K="473.16">1.4</Entry>
|
||||
<Entry Temperature_K="673.16">5.2</Entry>
|
||||
<Entry Temperature_K="873.16">19.5</Entry>
|
||||
</TemperatureVsWearCoefficientCurve>
|
||||
|
||||
</CoatingMaterial>
|
||||